斷裂伸長率 | 810% | 拉伸強度 | 40MPa | 密度 | 0.925g/cm3 |
熔體流動速率 | 0.65g/10min | 維卡軟化點 | 110℃ | 用途級別 | 薄膜級 |
規格級別 | 薄膜 | 特性級別 | 透明級 |
|
產品簡述
斷裂伸長率 | 810% | 拉伸強度 | 40MPa | 密度 | 0.925g/cm3 |
熔體流動速率 | 0.65g/10min | 維卡軟化點 | 110℃ | 用途級別 | 薄膜級 |
規格級別 | 薄膜 | 特性級別 | 透明級 |
詳細數據
訂購指南
性能項目 | 試驗條件[狀態] | 測試方法 | 測試數據 | 數據單位 | ||
基本性能 | 密度 | ASTM D-1505 | 0.925 | g/cm3 | ||
熔體流動速率 | ASTM D-1238 | 0.65 | g/10min | |||
物理性能 | 薄膜厚度 | 190 | µm | |||
機械性能 | 拉伸斷裂強度 | MD | ASTM D-882 | 440 | Kg/cm2 | |
TD | ASTM D-882 | 410 | Kg/cm2 | |||
撕裂強度 | MD | ASTM D-1004 | 130 | Kg/cm | ||
TD | ASTM D-1004 | 125 | Kg/cm | |||
斷裂伸長率 | MD | ASTM D-882 | 800 | % | ||
TD | ASTM D-882 | 810 | % | |||
尖頭沖擊強度 | ASTM D-3420 | 3.7 | g/μm | |||
拉伸屈服強度 | MD | ASTM D-882 | 150 | Kg/cm2 | ||
TD | ASTM D-882 | 145 | Kg/cm2 | |||
抗張模數 | MD | ASTM D-882 | 2600 | Kg/cm2 | ||
TD | ASTM D-882 | 3500 | Kg/cm2 | |||
熱性能 | 維卡軟化點 | ASTM D-1525 | 110 | ℃ | ||
低溫脆化溫度 | ASTM D-746 | <-80 | ℃ |